Some Features of Sintering of Tungsten Powders
Abstract
A method of activating the sintering process for tungsten powders using a closed reaction space and hydrogen, steam-saturated water was observed. This sintering process is allowed to activate super coarse-grained (1000 μm) tungsten powder sat relatively low temperatures (1000 - 1200 °C).
Downloads
Published
2017-12-13
Issue
Section
Articles
License
This work is licensed under a Creative Commons Attribution 4.0 International License.
Authors retain copyright of the published papers and grant to the publisher the right to publish the article, to be cited as its original publisher in case of reuse, and to distribute it in all forms and media. Articles will be distributed under the Creative Commons Attribution International License (CC BY 4.0).